Cell-Based Battery Health Measurement with EIS

An electric vehicle's battery pack consists of hundreds of cells, and not a single one of those cells is a copy of another. Manufacturing tolerances, temperature gradients, and differences in position within the pack cause each cell to age at its own pace. Here is the problem: the conventional BMS in the vehicle typically produces an SOH estimate at the pack level by monitoring the pack's total voltage and current; detecting a cell that has begun to wear out early only becomes possible once its effect becomes visible in the total. Electrochemical impedance spectroscopy, or EIS for short, on the other hand, brings this picture down to the cell level and can measure each cell's internal resistance individually while the battery is in operation.
On this page, we cover how EIS measures battery health cell by cell, why the passive method requires no additional hardware, and how cell-level digital passport frameworks such as CellPassport differ from conventional SOH estimation.
What Is EIS and How Is It Applied to a Cell?
Electrochemical impedance spectroscopy is a non-destructive diagnostic technique that applies a small-amplitude alternating current (AC) signal to a battery cell and measures the cell's voltage response. The signal is typically swept across a broad frequency range from 0.01 Hz to 100 kHz; at each frequency, the resistance the cell exhibits is different, because different frequencies activate different physical processes inside the cell. High frequencies reflect the conductivity of the electrolyte, mid frequencies the charge transfer at the electrode-electrolyte interface, and low frequencies ion diffusion.
The result is the impedance spectrum, which is usually visualized with two plots: the Nyquist plot, in which the real component of impedance is plotted against the imaginary component, and the Bode plot, in which the magnitude or phase angle is shown against frequency on a logarithmic scale. The Bode representation offers an advantage in distinguishing small impedance components alongside large ones. From the spectrum, parameters such as electrolyte resistance, double-layer capacitance, and charge transfer resistance are derived numerically; diffusion behavior is modeled with the Warburg impedance.
The critical point is this: the measurement does not harm the cell. The applied AC signal is small; there is no sampling or stressing of the battery involved. Contrary to destructive tests of the kind where you cannot learn the cell's character without questioning it, EIS provides information without touching the cell.
Passive EIS: Measuring with Charging Waves While the Battery Operates

Laboratory EIS relies on connecting the cell to a test device and injecting a controlled signal. The path for in-vehicle application is different: passive impedance spectroscopy uses the voltage and current profile that the battery itself generates. The current entering the battery during charging is inherently wavy; these fluctuations act as a continuous, perfect AC stimulus applied to the cell. The passive method records this profile in a synchronized manner and resolves each cell's impedance from the relationship between the voltage response and the current input.
The value of the approach is riveted by its mathematical framework. A study published in the Journal of Power Sources in 2020 proposed a passive framework for onboard impedance spectroscopy at the cell level without the need for additional hardware. As early as 2018, it had been shown that the impedance of a hybrid electric vehicle battery could be passively monitored and expanded over time and linked to SoC estimation with an unscented Kalman filter. So the idea is not new; As of 2026, what has changed is the maturity to do this inside series-production vehicles without adding measurement cost.
Highlights
- EIS measures cell impedance non-destructively with a small AC signal at frequencies between 0.01 Hz - 100 kHz.
- Passive EIS uses the battery's own charging waves and requires no additional hardware.
- New EIS-enabled battery monitoring chips can infer temperature, SoC and cell health without dedicated sensors.
- The cell-level digital passport experiment is being carried out publicly in an electric car by an OEM for the first time.
- Because EIS resolves impedance by frequency, it can show which degradation mechanism has started in which cell.
Why Is Internal Resistance the Most Honest Indicator of Health?
SOH is the ratio of the remaining maximum charge of the battery relative to its rated capacity: 100% in a new cell, dropping to roughly 80% as it approaches end of life. However, capacity is only the net outcome of aging. Internal resistance, on the other hand, tracks the process itself: as a cell ages, impedance increases and capacity decreases; in practice, a battery is considered degraded if it can deliver only 75% of its rated capacity. As resistance increases, a larger portion of the energy turns into heat; this heat puts degradation into a self-accelerating cycle.
Impedance is also sensitive to operating conditions: as SoC decreases (especially at low frequencies) impedance increases, and as temperature rises it decreases. Therefore, the value of cell-level measurement lies not in giving a single number, but in offering a fingerprint spread across the frequency axis. Each circuit element derived from the spectrum corresponds to a specific aging process: an increase in electrolyte resistance indicates electrolyte loss, and an increase in charge transfer resistance indicates deterioration at the electrode interface. Dynamic EIS studies published in 2026 have shown that this approach extends to the detection of a critical safety risk such as lithium plating.
Where Does It Differ from Pack-Level SOH Estimation?
Conventional health assessment methods (such as HPPC, DCIR, ICA) provide a general indicator of health decline; they cannot tell which cell has worn out through which mechanism. The OCV method requires a long rest period before measurement and is not suitable for onboard application; coulomb counting carries an error that accumulates over time. EIS, on the other hand, sees internal processes in detail, namely ion mobility, charge transfer, electrolyte conductivity and component degradation.
To draw an analogy: pack-level SOH is like looking only at the oil pressure light without analyzing the engine oil; when the lamp lights up, the damage has already been done. Cell-level impedance measurement, on the other hand, is like an analysis that counts the metal particles in the oil one by one. Since the increase in impedance directly reflects the rise in resistance at the electrode interfaces and in the electrolyte, degradation can be detected before performance loss becomes visible.
Another practical advantage of EIS is its chemistry independence: the method does not rely on pre-built models specific to a battery type, which makes it easy to adapt to different chemistries. Machine learning-based SoH models, however, may not perform reliably outside the chemistry they were trained on and require large, type-specific data sets. When EIS data is combined with machine learning, it becomes possible to identify degradation patterns, enabling early detection and remaining life estimation; a 2020 Nature Communications study in this area produced one of the most cited results in the field.
Comparison of the methods
| Method | What it measures | Limitation |
|---|---|---|
| HPPC | Resistance via pulse response | Long testing time, complex analysis |
| DCIR | DC internal resistance | Does not provide detailed health information |
| OCV | Open-circuit voltage | Requires rest time, low accuracy |
| EIS (passive) | Frequency-dependent impedance spectrum | Requires data interpretation tuning |
CellPassport and Cell-Level Digital Passports
Beyond measurement itself, organizing the data on a per-cell basis is a separate engineering challenge. CellPassport is described as a solution that transforms existing BMS data into per-cell diagnostics and impedance-based health indicators, providing a digital passport for each battery cell. The related project, carried out at Aalborg University, targets cloud-based, real-time cell diagnostics and lifecycle management using passive EIS. The workflow consists of four steps: synchronized data acquisition, quality control, diagnostic inference, and digital twin updates.
The most concrete example in the field came from Kia: Kia became the first manufacturer to publicly test a cell-level battery passport in an electric car; in the trial, monitoring chips attached to each cell could store cell-based SoH data on the chip itself, providing live health tracking, real-time repair diagnostics, and end-to-end traceability. This is also an architecture compatible with the EU Battery Passport legislation's principle of storing identity, production, and operational data at the source; 2027 is targeted for the launch of the Global Battery Alliance's global passport scheme.
2026 in the Field: E-Buses and New BMS Chips
The hardware side is maturing rapidly. Texas Instruments introduced its BQ79826-Q1 battery monitor, announced in June 2026, with EIS support, positioning it as the industry's highest cell-count EIS battery tracker; the chip's standout capability is its ability to derive battery temperature, SoC, and cell health from impedance data without dedicated temperature sensors. NXP aims to improve battery health monitoring, EV safety and fast charging performance with its EIS-capable cell monitoring chipset. On the cell production line side, there are integrated solutions where a single EIS test device supports up to 72 channels; the technology's coverage extends from production all the way into the vehicle.
The gains are even more visible in fleet operations. In 2026 e-bus maintenance practice, charging management, battery health monitoring, thermal control and lifecycle tracking are among the priority topics; an e-bus battery is the largest cost item per vehicle, and the early degradation of a single cell can render the entire package out of service. In-situ applications demonstrating the feasibility of real-time impedance measurement at EV scale have also found their place in the literature. On the market side, the EV battery health monitoring market is expected to grow from 8.1 billion US dollars in 2025 to 25.6 billion dollars in 2035, at a compound annual growth rate of 12.2%; such projections should be approached with caution, treating them as secondary market reports.
Limitations and an Honest Look
EIS is not a silver bullet. The semicircles in Nyquist plots can overlap; this makes it unclear which electrochemical process is responsible during degradation. For the solution, combinations of distribution of relaxation times (DRT) analysis and machine learning are proposed; in recent years, models combined with autoencoders and correlation analysis have outperformed previous neural network models on four lithium-ion batteries at three different temperatures. In addition, the literature on applying EIS in EVs is still relatively scarce; findings transferred from general battery research cannot always be directly carried over to in-vehicle conditions.
Short Answer: How Does Cell-by-Cell Health Measurement Work with EIS?
In summary: passive EIS extracts a frequency-based impedance spectrum for each cell by resolving the relationship between the alternating current sent to the cells while the battery is charged normally and the voltage response; from this spectrum, internal resistance, charge transfer resistance and electrolyte conductivity are derived, and which degradation mechanism has started in which cell is read before performance loss becomes visible. At pack level, classic SOH estimation reports the result; at cell level, passive EIS reports the process. The difference is as practical as the difference between a repair bill and planned maintenance.